Short- and Long-Term Bond Strength Between Resin Cement and Glass-Ceramic Using a Silane-Containing Universal Adhesive

This study aimed to evaluate the effect of various silane-containing solutions on bonding between resin cement and glass ceramic after 24 hours and after six months of water storage. Glass-ceramic plaques (IPS e.max CAD) were sandblasted with aluminum oxide, etched with 10% hydrofluoric acid (HF), a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Operative dentistry 2017-09, Vol.42 (5), p.514-525
Hauptverfasser: Murillo-Gómez, F, Rueggeberg, F A, De Goes, M F
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This study aimed to evaluate the effect of various silane-containing solutions on bonding between resin cement and glass ceramic after 24 hours and after six months of water storage. Glass-ceramic plaques (IPS e.max CAD) were sandblasted with aluminum oxide, etched with 10% hydrofluoric acid (HF), and divided into five "silane treatment" groups: RelyX Ceramic Primer (RCP), RelyX Ceramic Primer and Single Bond Plus (RCP+SB), Scotchbond Universal (SBU), Clearfil Ceramic Primer (CP), and no solution (HF-only control). Each group was divided into two "storage time" subgroups: 24 hours or six months in 37°C water. Eighteen resin cement cylinders (RelyX Ultimate) were bonded to each treatment group substrate (n=18) and then subjected to microshear testing. Failure mode was analyzed using scanning electron microscopy. Debond data were analyzed using a two-way analysis of variance and the Tukey post hoc test (α=0.05) as well as Weibull distributions. The factors "silane treatment," "storage time," (p