Determining the Coefficients of Fusion and of Weld Deposition at Mechanized Mag-C Welding with Solid Wire and Cored Wires

In the case of the MAG welding of carbon and low-alloyed steels wires or hollow wires with (rutilic or basic) flux with metallic powder or self-protection are used. In indoors weldings huge quantities of smoke, gases, dust and particles in suspension, etc. get accumulated. These noxious substances p...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied Mechanics and Materials 2014-10, Vol.657 (Engineering Solutions and Technologies in Manufacturing), p.301-305
Hauptverfasser: Mihăilescu, Dănuţ, Georgescu, Bogdan, Gheonea, Marius Cornel
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In the case of the MAG welding of carbon and low-alloyed steels wires or hollow wires with (rutilic or basic) flux with metallic powder or self-protection are used. In indoors weldings huge quantities of smoke, gases, dust and particles in suspension, etc. get accumulated. These noxious substances produced during the welding process may severely affect the welders health. To improve the welders working conditions, on an international scale, the following are used: welding masks with self-obscurazation and air control; noxious substances vacuum cleaners fitted with filters; MAG welding pistols with gase and smoke absorbing devices. For the improvement of the welders working conditions, producers of welding materials invented hollow wires with (rutilic flux or with metallic powder) with a smoke-reduced emission [1,2,3,4,5].
ISSN:1660-9336
1662-7482
1662-7482
DOI:10.4028/www.scientific.net/AMM.657.301