Investigation of Defects Accumulation in the Process of Hydrogen Sorption and Desorption
This paper is devoted to the defect structure study of commercially pure titanium after hydrogen sorption-desorption cycles by means of positron lifetime (PL) and Doppler broadening spectrometry. Material was loaded with hydrogen from the gas phase till the concentration of hydrogen reached the valu...
Gespeichert in:
Veröffentlicht in: | Advanced Materials Research 2015-02, Vol.1085, p.328-334 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This paper is devoted to the defect structure study of commercially pure titanium after hydrogen sorption-desorption cycles by means of positron lifetime (PL) and Doppler broadening spectrometry. Material was loaded with hydrogen from the gas phase till the concentration of hydrogen reached the value of 0.05 wt.% for each cycle. The essential changes in the positron annihilation characteristics of the sample are occurred after the each stage of treatment. |
---|---|
ISSN: | 1022-6680 1662-8985 1662-8985 |