Synthesis and structures of bis-ligated zinc complexes supported by tridentate ketoimines that initiate L-lactide polymerization

Eight bis-ligated, homoleptic, zinc complexes were synthesized through the reaction of NNO Schiff base ketoimines bearing varying substituents with diethyl zinc in an inert atmosphere glovebox at room temperature and isolated in 62-95% yield. The complexes were characterized with (1)H, (13)C, and (1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Dalton transactions : an international journal of inorganic chemistry 2014-11, Vol.43 (43), p.16498-16508
Hauptverfasser: Gerling, Kimberly A, Rezayee, Nomaan M, Rheingold, Arnold L, Green, David B, Fritsch, Joseph M
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Eight bis-ligated, homoleptic, zinc complexes were synthesized through the reaction of NNO Schiff base ketoimines bearing varying substituents with diethyl zinc in an inert atmosphere glovebox at room temperature and isolated in 62-95% yield. The complexes were characterized with (1)H, (13)C, and (19)F nuclear magnetic resonance spectroscopy, absorbance spectroscopy, high resolution mass spectrometry, elemental analysis, and single crystal X-ray crystallography. The complexes were shown to adopt distorted octahedral coordination geometry around zinc. The (1)H and (19)F NMR spectra of complexes 1-7 showed stable zinc coordination at 300 K while the effect of steric encumbrance and two trifluoromethyl groups in complex 8 was investigated with variable temperature NMR. The bis-ligated zinc complexes were effective initiators for the ring opening polymerization of L-lactide into poly-L-lactic acid (PLLA). With [L-lac]/[Zn complex] = 50, the bis-ligated zinc complexes yielded percentage conversion of 14-98% with polymerization times varying from 15-1440 min, where the longest reaction times were required when two trifluoromethyl groups were present. The addition of 4-fluorophenol co-catalyst resulted in up to a 5-fold increase in the percentage conversion in toluene solution and up to a 14-fold increase in bulk melt polymerization with reductions in the poly-dispersity index values for the isolated PLLA. Addition of 4-fluorophenol to complex 1 was studied with (1)H and (19)F NMR and appeared to yield an in situ generated zinc alkoxide complex.
ISSN:1477-9226
1477-9234
DOI:10.1039/c4dt01607f