Effects of different surface treatments on stainability of ceramics

Statement of problem Final adjustments may result in a loss of ceramic glaze, a situation which must be corrected by reglazing or polishing to obtain clinically successful restorations; such restorations may be susceptible to staining. Purpose The purpose of this study was to determine the stainabil...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:The Journal of prosthetic dentistry 2012-10, Vol.108 (4), p.231-237
Hauptverfasser: Motro, Pelin F. Karagoz, DDS, MSc, Kursoglu, Pınar, DDS, PhD, Kazazoglu, Ender, DDS, PhD
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Statement of problem Final adjustments may result in a loss of ceramic glaze, a situation which must be corrected by reglazing or polishing to obtain clinically successful restorations; such restorations may be susceptible to staining. Purpose The purpose of this study was to determine the stainability of ceramics exposed to coffee after different surface treatments and to correlate the surface roughness with the color differences. Material and methods Sixty-six ceramic (IPS e.maxCeram) disks (15 × 2 mm) were fabricated and glazed according to the manufacturer's instructions, then assigned to 6 groups. Group Glaze (Group G), the control, was not subjected to any procedure. All the others were abraded with a diamond rotary cutting instrument. Group Reglaze (Group R) was reglazed; others were polished with different polishing materials; Group Shofu (Group S) was polished with abrasive stone (Dura-Green Stones), coarse silicon polisher (Ceramaster Coarse), silicon polisher (CeraMaster), and polishing paste (Ultra II) with polishing disks (Super-Snap Buff Disks); Group Ultradent (Group U) was polished with 1.0 and 0.5-μm polishing pastes (Ultradent Diamond) with a goat hair brush (Jiffy) and Group Bredent (Group B) was polished with an abrasive stone (Diagen turbo grinder), a round polishing brush (Abraso-fix), and polishing paste (Diamond) with felt wheels. Group Diamond rotary cutting instrument (Group D) was not treated after abrasion with a diamond rotary cutting instrument. Surface roughness was evaluated by profilometer (n=10), and 1 specimen from each group was evaluated by scanning electron microscopy (SEM). Color difference was measured by a spectrophotometer before and after 12 days of immersion in a coffee solution. Data were analyzed by 1-way ANOVA, the Tukey HSD test, and the Pearson rank correlation tests (α=.05). Results The surface roughness (Ra) values were ordered from the highest to the lowest value, which were Group D, B, U, S, R, and G, respectively. Significant differences among groups ( P