Recovery of iron from copper slag by deep reduction and magnetic beneficiation

Aiming at recovering iron from high-iron-content copper slag, this article introduced a combination technol- ogy of deep reduction and magnetic beneficiation, investigated the iron recovery efficiency and optimized the technical conditions. When coke powder with 86wt% fixed carbon was used as a redu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of minerals, metallurgy and materials metallurgy and materials, 2013-11, Vol.20 (11), p.1035-1041
Hauptverfasser: Li, Ke-qing, Ping, Shuo, Wang, Hong-yu, Ni, Wen
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Aiming at recovering iron from high-iron-content copper slag, this article introduced a combination technol- ogy of deep reduction and magnetic beneficiation, investigated the iron recovery efficiency and optimized the technical conditions. When coke powder with 86wt% fixed carbon was used as a reductant, iron was successfully extracted from the copper slag. Under the optimized condition of the coke powder content of 14wt%, the calcium-to-silicon mass ratio (Ca/Si) of 0.2, the roasting temperature of 1300℃, the roasting time of 3 h, the grinding time of 20 min, and the magnetic field intensity of 61 kA-m-1, the iron recovery rate of the copper slag can reach 91.82%, and the extracted iron powder has an iron grade of 96.21%. With the characteristics of high iron grade and low impurity content, the extracted iron powder can be used as high-quality raw materials of weathering steel.