Preparation of the PBOPy/PPy/Fe sub(3)O sub(4) composites with high microwave absorption performance and thermal stability
A microwave absorption composite is prepared by polypyrrole (PPy) coated Fe sub(3)O sub(4) magnetic nano-particles and pyridine-based polybenzobisoxazole (PBOPy) by the means of solution blending. Fourier transform infrared spectroscopy. X-ray diffraction, transmission electron microscopy, scanning...
Gespeichert in:
Veröffentlicht in: | Composites science and technology 2014-01, Vol.100, p.212-219 |
---|---|
Hauptverfasser: | , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A microwave absorption composite is prepared by polypyrrole (PPy) coated Fe sub(3)O sub(4) magnetic nano-particles and pyridine-based polybenzobisoxazole (PBOPy) by the means of solution blending. Fourier transform infrared spectroscopy. X-ray diffraction, transmission electron microscopy, scanning electron microscopy-energy dispersive spectrometer, vibrating-sample magnetometry, and thermogravimetric analysis are employed to investigate properties of the prepared composites. Composites behave good thermal stability (high char yield above 60 wt%, 800 [degrees]C, in nitrogen). The magnetic saturation of PPy/ Fe sub(3)O sub(4) is 17.94 emu/g, and that of PBOPy/PPy/Fe sub(3)O sub(4) composite is 0.36 emu/g. Vector network analyzer is used to measure electromagnetic parameters of PBOPy/PPy/Fe sub(3)O sub(4) composite. Reflection losses (RL (dB)) are calculated in the frequency range of 2-18 GHz. PBOPy/PPy/Fe sub(3)O sub(4) composite with 8 wt% PPy/ Fe sub(3)O sub(4) behaves a minimum RL vaiue of -23.3 dB and below -10 dB in 11.6-13.84 GHz at the film thickness with 3.5 mm. |
---|---|