Obtainment of the Fe0.70−xCrxAl0.3/Al2O3 nanocomposite by the method of SHS of mechanoactivated Cr2O3 + Fe + Al mixtures

Applying Mössbauer spectroscopy methods, we have studied the structure of nanocomposites obtained by a technique combining the preliminary mechanical activation of an 8.1 wt % Cr 2 O 3 + 65.9 wt % Fe + 25 wt % Al mixture and self-propagating high-temperature synthesis (SHS). It has been found that,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Inorganic materials 2009-07, Vol.45 (7), p.827-831
Hauptverfasser: Kiseleva, T. Yu, Novakova, A. A., Talako, T. L., Grigor’eva, T. F., Falkova, A. N.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Applying Mössbauer spectroscopy methods, we have studied the structure of nanocomposites obtained by a technique combining the preliminary mechanical activation of an 8.1 wt % Cr 2 O 3 + 65.9 wt % Fe + 25 wt % Al mixture and self-propagating high-temperature synthesis (SHS). It has been found that, at the stage of mechanical activation, an Fe/Al/Cr 2 O 3 composite with a low impurity of the Fe 2 Al 5 intermetallide is formed. At the stage of SHS, the interaction between activated components of the mixture leads to the formation of the Fe 0.7 − x Cr x Al 0.3 ( x = 0 − 0.2)/Al 2 O 3 composite.
ISSN:0020-1685
1608-3172
DOI:10.1134/S002016850907022X