The effects of hardpan layers on the water chemistry from the leaching of pyrrhotite-rich tailings material

Column leaching experiments were used to determine the effects of an iron-rich hardpan layer, on the rate of tailings oxidation and the composition of leachate waters, from the Renison Bell tailings dams in western Tasmania, Australia. One-meter-long PVC columns, filled with tailings, cover material...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Environmental earth sciences 2003-09, Vol.44 (6), p.687-697
Hauptverfasser: GILBERT, S. E, COOKE, D. R, HOLLINGS, P
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Column leaching experiments were used to determine the effects of an iron-rich hardpan layer, on the rate of tailings oxidation and the composition of leachate waters, from the Renison Bell tailings dams in western Tasmania, Australia. One-meter-long PVC columns, filled with tailings, cover material (Cassiterite Flotation Tailings) and hardpan samples from the tailings dams, were leached over a period of 14 weeks. Under dry cover conditions, when hardpan was present, the solute loads peaked at 21-49 days (Fe at 2,294 ppm and SO^sub 4^^sup 2-^ at 4,700 ppm), and stabilised at much lower concentrations after 9 weeks. In contrast, the solute loads steadily increased over time in the column where hardpan was absent (SO^sub 4^^sup 2-^ from 1,800 to 3,100 ppm, and Fe from 407 to 1,692 ppm). Under saturated cover conditions, the solute concentrations in the leachate also increased with time (SO^sub 4^^sup 2-^from 1,900 to 17,000 ppm, and Fe from 480 to 8,500 ppm). The presence of a hardpan layer between the reactive tailings and cover material has been found to improve leachate water chemistry and lessen the rate of sulphide oxidation.[PUBLICATION ABSTRACT]
ISSN:0943-0105