Effects of ammonia concentration on property of Cd sub(1-x)Zn sub(x)S films by chemical bath deposition

Cd sub(1-x)Zn sub(x)S thin films were grown on soda-lime glass substrates by chemical-bath deposition (CBD) at 80 degree C with stirring. All the samples were annealed at 200 degree C for 60 min in the air. The crystal structure, surface morphology, thickness and optical properties of the films were...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science in semiconductor processing 2014-03, Vol.19, p.78-82
Hauptverfasser: Dong, Yuejie, Zhou, Limei, Wu, Sumei
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Cd sub(1-x)Zn sub(x)S thin films were grown on soda-lime glass substrates by chemical-bath deposition (CBD) at 80 degree C with stirring. All the samples were annealed at 200 degree C for 60 min in the air. The crystal structure, surface morphology, thickness and optical properties of the films were studied with transmission electron microscopy (TEM), X-ray diffraction (XRD), scanning electron microscopy (SEM), step height measurement instrument and spectrophotometer respectively. The results revealed that Cd sub(1-x)Zn sub(x)S thin films had cubic crystal structure and the intensity of the diffraction peak increased gradually as ammonia concentration rose and the grain size varied from 5.1 to 8.3 nm. All of Cd sub(1-x)Zn sub(x)S thin films had a granular surface with some smaller pores and the average granule sizes increased from 92 to 163 nm with an increase in ammonia concentration. The Cd sub(1-x)Zn sub(x)S thin films had the highest transmittance with ammonia concentration of 0.5 M L super(-1), whose thickness was 50 nm and band gap was 2.62 eV.