Degradation and deactivation of Sn catalyst used for CO sub(2) reduction as function of overpotential

Degradation and deactivation mechanisms of an Sn catalyst used for CO sub(2) reduction to formate in 2 M KCl solution was investigated at various potentials by using a rotating disk electrode. Surface degradation was studied by SEM/EDS and chemical analysis was performed by XPS. The results indicate...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Electrochimica acta 2014-07, Vol.133, p.188-196
Hauptverfasser: AnawatiFrankel, G S, Agarwal, Arun, Sridhar, Narasi
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Degradation and deactivation mechanisms of an Sn catalyst used for CO sub(2) reduction to formate in 2 M KCl solution was investigated at various potentials by using a rotating disk electrode. Surface degradation was studied by SEM/EDS and chemical analysis was performed by XPS. The results indicated that the optimum potential for CO sub(2) reduction on Sn electrode was similar to -1.8 V sub(SCE) where maximum faradaic efficiency and minimum degradation were obtained. Two types of degradation were observed after cathodic polarization: cathodic corrosion resulting in the potential loss of catalyst and formation of alkali metal deposits resulting in deactivation of the catalyst. The former type gave a crystallographic type of etching morphology near and at the grain boundaries after polarization in the potential range of -1.8 to -2.2 V sub(SCE). The number of attacked areas increased at more negative potentials and with increasing electrode rotation rate. Corrosion did not cause electrode deactivation as indicated by a relatively stable faradaic efficiency. Moreover, the material loss was insignificant because only small areas were affected. Corrosion was attributed to the formation of tin hydride. Meanwhile, formation of intermetallic compound (KSn), which occurred during simultaneous CO sub(2) reduction reaction at all potentials tested in this work, led to both cathodic deactivation and material loss. The existence of KSn deposits on the electrode surface was detected by EDS. The formation of intermetallic compound was always accompanied by an increase in current output possibly due to hydrogen evolution. Heavy colloidal deposits of KSn were found. For use of an Sn catalyst in a device, it is necessary to develop a technique to avoid or remove the alkali metal deposit.
ISSN:0013-4686
DOI:10.1016/j.electacta.2014.04.057