Effect of accelerated aging on the bonding performance of fluoridated adhesive resins

The purpose of this study was to investigate the dentin bond durability of a one-step, fluoride-containing, glass ionomer-based adhesive system, Reactmer Bond (RB), and that of a two-step, fluoride-containing, self-etch adhesive system, Clearfil Protect Bond (CPB). Enamel was removed from the occlus...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Dental Materials Journal 2014/01/30, Vol.33(1), pp.92-97
Hauptverfasser: COBANOGLU, Nevin, OZTURK, Bora, SENGUN, Abdulkadir, CETİN, Ali Riza, OZER, Fusun
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The purpose of this study was to investigate the dentin bond durability of a one-step, fluoride-containing, glass ionomer-based adhesive system, Reactmer Bond (RB), and that of a two-step, fluoride-containing, self-etch adhesive system, Clearfil Protect Bond (CPB). Enamel was removed from the occlusal surfaces of teeth, and flat dentin surfaces were entirely covered with a composite resin following the application of an adhesive material (n=10). After specimens were sectioned into rectangular sticks of 0.87±0.03 mm2, the sticks were randomly assigned into two accelerated aging time period groups: 1 week or 1 year. Microtensile bond strengths were determined. Bond strength of RB increased significantly after 1 year (1 week=27.80±10.57 MPa versus 1 year=36.93±14.38 MPa) (p0.05). Both fluoride-containing adhesives seemed to demonstrate reliable bonding performance after 1 year of accelerated aging in water.
ISSN:0287-4547
1881-1361
DOI:10.4012/dmj.2013-107