Preparing With Excessive Mg Environment Sintering and Two-Step Sintering Approach
MgB 2 superconductors were made with two processes in this work. In one case, the SiC doped MgB 2 pellets were sintered in excessive Mg medium. It is found that the samples sintered in excessive Mg medium present Mg-rich composition comparing with the one sintered in Ar gas. The density is higher an...
Gespeichert in:
Veröffentlicht in: | IEEE transactions on applied superconductivity 2009-06, Vol.19 (3), p.2748-2751 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | MgB 2 superconductors were made with two processes in this work. In one case, the SiC doped MgB 2 pellets were sintered in excessive Mg medium. It is found that the samples sintered in excessive Mg medium present Mg-rich composition comparing with the one sintered in Ar gas. The density is higher and the resistance is lower due to the penetration of the Mg into the pores and grain boundary of MgB 2 , which is beneficial to the J c improvement. In the other case, a two-step process was employed to make MgB 2 . J c of the sample with the composition of MgB 4 is very low after the first sintering. The J c was dramatically improved after the second sintering, but J c of the two-step made sample is still poorer than the MgB 2 made with general one step sintering due to the connectivity deterioration caused by the pulverization prior to the second sintering. |
---|---|