The work hardening model of dual-phase Mg–8Li–3Al–1Nd alloy

The work hardening behavior of dual-phase Mg–8Li–3Al–1Nd alloy sheet is investigated at 293–473 K with a strain rate of 0.083–0.00083 s −1 . Experiment results show that the flow stress is sensitive to deformation conditions, and decreased with the increased of temperature and the reduced of strain...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science 2024-08, Vol.59 (31), p.14593-14605
Hauptverfasser: Dai, Zhengkun, Li, Xialei, Zhou, Haitao
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The work hardening behavior of dual-phase Mg–8Li–3Al–1Nd alloy sheet is investigated at 293–473 K with a strain rate of 0.083–0.00083 s −1 . Experiment results show that the flow stress is sensitive to deformation conditions, and decreased with the increased of temperature and the reduced of strain rate. On the basis of flow stress curves, the work hardening behavior is analyzed as work hardening rate ( θ ) with net flow stress ( σ - σ y ) and true strain ( ε p ) curves, which is defined as four stages: stage II (linear hardening stage), stage III and IV (softening stage), stage V (late deformation stage), but the work hardening stage II only occurs under certain conditions. The stage II, III and IV can be expressed by three models. By the models, the work hardening rate can be predicated.
ISSN:0022-2461
1573-4803
DOI:10.1007/s10853-024-10001-2