The Effect of Alkaline Concentration and Curing Temperature on the Durability of Fly Ash Geopolymer Mortar

In this study, fly ash was used to synthesize geopolymer mortar by using an activating solution prepared from a different concentration of NaOH and a highly viscous Na-silicate. The NaOH concentration prepared were 8M, 12M, and 14M. The prepared geopolymers were cured at different temperatures (ambi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Advanced materials research 2022-06, Vol.1172, p.95-107
Hauptverfasser: Ourgessa, Abel Woldu, Tasew, Aseged Tebeje, Hafa, Rahel Alemu
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this study, fly ash was used to synthesize geopolymer mortar by using an activating solution prepared from a different concentration of NaOH and a highly viscous Na-silicate. The NaOH concentration prepared were 8M, 12M, and 14M. The prepared geopolymers were cured at different temperatures (ambient, 40°C, and 60°C) and were studied to determine their strength, bond structure, mechanical properties, and resistance in an acidic and salty environment using an accelerated durability test. FTIR results showed distinctive peaks of aluminosilicate bond structures. Maximum strength was achieved for 14M samples cured at room temperature. Higher alkalinity resulted in higher compressive and flexural strength and lower water absorption. Lower water absorption capacity and higher resistance to the extreme environment were achieved for samples cured at higher temperatures and higher molarities. The maximum mass loss was 10.9% for 8M cured at ambient temperature exposed to an acidic environment.