Competing High-Temperature Deformation Mechanisms in Mo(Si,Al)2–Al2O3 Composites

Mo(Si,Al) 2 –Al 2 O 3 composites were tested in four-point bending at 1300 °C. The addition of Al 2 O 3 led to a decrease in grain size, and a subsequent decrease in strength for materials containing up to 15 wt pct Al 2 O 3 . At higher Al 2 O 3 fractions, the decrease in grain size saturates and th...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Metallurgical and materials transactions. A, Physical metallurgy and materials science Physical metallurgy and materials science, 2024-09, Vol.55 (9), p.3220-3225
Hauptverfasser: Edgren, Aina, Ström, Erik, Colliander, Magnus Hörnqvist
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Mo(Si,Al) 2 –Al 2 O 3 composites were tested in four-point bending at 1300 °C. The addition of Al 2 O 3 led to a decrease in grain size, and a subsequent decrease in strength for materials containing up to 15 wt pct Al 2 O 3 . At higher Al 2 O 3 fractions, the decrease in grain size saturates and the strength is recovered as the Al 2 O 3 particles prevent grain boundary sliding.