Investigation Into the Possibility of Intensifying the Sintering of Pure Magnesia Raw Materials

The influence of additives of different nature on grinding, compressibility, and sintering of calcined magnesite was investigated. It was found that the investigated recycled additives, when introduced in the amount of up to 0.5 wt.%, have no significant effect on the grain composition of calcined p...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Refractories and industrial ceramics 2024, Vol.64 (5), p.517-520
Hauptverfasser: Fayruzov, K. V., Kashcheev, I. D., Zemlyanoy, K. G.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The influence of additives of different nature on grinding, compressibility, and sintering of calcined magnesite was investigated. It was found that the investigated recycled additives, when introduced in the amount of up to 0.5 wt.%, have no significant effect on the grain composition of calcined periclase after grinding, the compressibility of powders, and their chemical and phase composition after firing at a temperature of up to 1870°C. An additive based on dust wastes of titanium production enables increasing the density of the obtained briquette by 1.0 – 3.5 % or reducing the briquette firing temperature by 50 – 100°C.