Performance Evaluations of Warm-Mix Reaction-Rejuvenated SBS Modified Asphalt Mixtures Incorporated with Wax-Based Additive

The high-performance, cleaner rejuvenation of aged SBS-modified asphalt mixtures (ASBSMAMs) has been a hotspot in asphalt research. Currently, the most popular rejuvenation method still involves hot-mix asphalt with a commonly used oil as the rejuvenator for recycling. However, high-quality, cleaner...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Sustainability 2024-06, Vol.16 (12), p.5234
Hauptverfasser: Liu, Zihui, Chen, Qi, Pei, Junwen, Wang, Ruiyang, Shen, Weili, Huang, Chao, Liu, Jialiang, Xu, Xiong
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The high-performance, cleaner rejuvenation of aged SBS-modified asphalt mixtures (ASBSMAMs) has been a hotspot in asphalt research. Currently, the most popular rejuvenation method still involves hot-mix asphalt with a commonly used oil as the rejuvenator for recycling. However, high-quality, cleaner warm-mix rejuvenation technology for ASBSMAMs is still needed to enrich this field. This study considered adopting a polyurethane (PU) prepolymer and 1,4-butanediol diglycidyl ether (BUDGE) as reactive rejuvenators to achieve warm-mix reaction–rejuvenation to enhance the properties of ASBSMAMs with the use of a wax-based additive, Sasobit. A series of tests were conducted to realize this, including the viscosity–temperature correlation of the rejuvenated binders, as well as tests of the moisture-induced damage, high-temperature stability, low-temperature cracking resistance, and fatigue resistance of the rejuvenated mixtures. The results showed the following: through reaction–rejuvenation, Sasobit could reduce the viscosity of the rejuvenated SBSMA (RSBSMA) below 150 °C for warm mixing and slightly decrease the viscosity–temperature susceptibility; warm-mix reaction–rejuvenation helped to improve the resistance to water-immersion-induced damage and freeze–thaw damage in ASBSMAMs; the addition of Sasobit showed benefits in improving their resistance to permanent deformation, with the dynamic stability values exceeding 5700 pass/mm as more than 1% Sasobit was added; the flexural damage resistance of ASBSMAMs at low temperatures could be enhanced after warm-mix reaction–rejuvenation; and, under reaction–rejuvenation conditions, Sasobit did not reduce the fatigue resistance of the RSBSMAM and, conversely, at limited higher dosages, it worked more effectively. Overall, the studied warm-mix reaction–rejuvenation technology has been proven to be effective for the environmental recycling and reuse of ASBSMAMs at high quality.
ISSN:2071-1050
2071-1050
DOI:10.3390/su16125234