Wear resistance and friction coefficient of nano-SiO2 and ash-filled HDPE/lignocellulosic fiber composites

This work comparatively evaluates the effect of nano-SiO 2 (at 2 and 3 wt%), rice husk and bagasse ash (at 5 and 10 wt%) on the wear resistance and friction coefficient of HDPE (high-density polyethylene)/lignocellulosic fiber composites. Rice husk and bagasse fibers at 50% by weight contents were m...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Polymer bulletin (Berlin, Germany) Germany), 2017-11, Vol.74 (11), p.4537-4547
Hauptverfasser: Sheykh, Mohammad Javad, Tarmian, Asghar, Doosthoseini, Kazem, abdulkhani, Ali
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This work comparatively evaluates the effect of nano-SiO 2 (at 2 and 3 wt%), rice husk and bagasse ash (at 5 and 10 wt%) on the wear resistance and friction coefficient of HDPE (high-density polyethylene)/lignocellulosic fiber composites. Rice husk and bagasse fibers at 50% by weight contents were mixed with HDPE and 2% maleic anhydride-grafted polyethylene as compatibilizer. SEM images showed a fairly appropriate connection between the polymer matrix and fillers. We found that the fillers improve the wear resistance, and the effect of nano-SiO 2 is more pronounced. The rice husk ash showed a better performance compared to the bagasse ash, probably due to greater SiO 2 content measured by X-ray fluorescence spectrometry. In contrast to nano-SiO 2 , both ashes had a reducing effect on other mechanical strengths (Izod impact resistance, modulus of elasticity and modulus of rupture). All fillers remarkably increased the water absorption and thickness swelling. The water uptake of composites increased after wear.