Extraction of Potassium from Feldspar by Roasting with CaCl2 Obtained from the Acidic Leaching of Wollastonite-Calcite Ore

Potassium, which is included in certain contents in the structure of K-feldspar minerals, has a very important function in the growth of plants. Turkey hosts the largest feldspar reserves in the world and is by far the leader in feldspar mining. The production of potassium salts from local natural s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Minerals (Basel) 2021-12, Vol.11 (12), p.1369
Hauptverfasser: Türk, Tülay, Üçerler, Zeynep, Burat, Fırat, Bulut, Gülay, Kangal, Murat Olgaç
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Potassium, which is included in certain contents in the structure of K-feldspar minerals, has a very important function in the growth of plants. Turkey hosts the largest feldspar reserves in the world and is by far the leader in feldspar mining. The production of potassium salts from local natural sources can provide great contributions both socially and economically in the agriculture industry along with glass production, cleaning materials, paint, bleaching powders, and general laboratory purposes. In this study, potassium extraction from K-feldspar ore with an 8.42% K2O content was studied using chloridizing (CaCl2) roasting followed by water leaching. Initially, to produce wollastonite and calcite concentrates, froth flotation tests were conducted on wollastonite-calcite ore after comminution. Thus, wollastonite and calcite concentrates with purities of 99.4% and 91.96% were successfully produced. Then, a calcite concentrate was combined with hydrochloric acid (HCl) under optimal conditions of a 1 mol/L HCl acid concentration, a 60 °C leaching temperature, and a 10 min leaching time to produce CaCl2. To bring out the importance of roasting before the dissolution process, different parameters such as roasting temperature, duration, and feldspar—CaCl2 ratios were tested. Under optimal conditions (a 900 °C roasting temperature, a 60 min duration, and a 1:1.5 feldspar—CaCl2 ratio), 98.6% of the potassium was successfully extracted by the water leaching process described in this article.