Luminescence Properties of Co-doped Eu3+, Bi3+ Lu2O3/Polyvinylpyrrolidone Films
The effect of the polyvinylpyrrolidone (PVP, MW = 130,000) molar content, PVP/Lu = 1, 2.5, 4 and 5; on the photoluminescent and structural properties of sol-gel derived Lu2O3:Eu3+, Bi3+ has been analyzed. Thin hybrid films were deposited by means of the dip-coating technique on silica quartz substra...
Gespeichert in:
Veröffentlicht in: | Coatings (Basel) 2018-11, Vol.8 (12), p.434 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The effect of the polyvinylpyrrolidone (PVP, MW = 130,000) molar content, PVP/Lu = 1, 2.5, 4 and 5; on the photoluminescent and structural properties of sol-gel derived Lu2O3:Eu3+, Bi3+ has been analyzed. Thin hybrid films were deposited by means of the dip-coating technique on silica quartz substrates. Films deposited at 700 °C presented a cubic structure, with non-preferential orientation, even with the presence of PVP. The photoluminescence (PL) spectrum and Comission Internationale de l’Éclairage (CIE) chromaticity diagram of films revealed a reddish Eu3+ emission at 612 nm (5D0 →7F2) with an excitation at 320 nm of the Bi ions (6s2→6s6p), showing a highly-effective energy transfer process form Bi3+ to Eu3+ luminescent centers. On the other hand, the color temperature of the samples is strongly dependent on the PVP content, as a consequence of the observed difference on the branching ratios of 5D0 →7FJ transitions of europium ions. Lifetime studies present two different behaviors for the thin films: A non-exponential nature for the lower PVP contents, and a simple exponential nature for the highest PVP one, showing that the PVP tends to promote a better dissolution of segregates and, therefore, increases the lifetime of the Eu3+ emission. |
---|---|
ISSN: | 2079-6412 2079-6412 |
DOI: | 10.3390/coatings8120434 |