Effects of eucommia gum filler on the dielectric properties and chemical resistances of addition-cure liquid silicone rubber
It is of great interest and remains a challenge to simultaneously improve the low dielectric properties and chemical resistances of addition-cure liquid silicone rubber (ALSR). In this work, we proposed an efficient approach to address this issue by filling silicone-modified Eucommia ulmoides gum na...
Gespeichert in:
Veröffentlicht in: | Journal of materials science. Materials in electronics 2021-08, Vol.32 (15), p.20548-20558 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | It is of great interest and remains a challenge to simultaneously improve the low dielectric properties and chemical resistances of addition-cure liquid silicone rubber (ALSR). In this work, we proposed an efficient approach to address this issue by filling silicone-modified
Eucommia ulmoides
gum nanofiller (SEUG) into ALSR. By adding 5 wt% SEUG, the dielectric constant of the SEUG/ALSR composite rubber was significantly lower than that of neat ALSR both at 10
2
Hz, 10
3
Hz, and 10
4
Hz. Simultaneously, the SEUG/ALSR composite rubber exhibited better mechanical and insulation properties than the neat ALSR after HCl, NaCl, and oil resistance tests. Our findings demonstrated the great potential for fabricating silicone rubber with low dielectric properties and erosion resistance by the utilization of natural biomass rubber material, endowing it with excellent mechanical performance and degradability. |
---|---|
ISSN: | 0957-4522 1573-482X |