CRACK INVESTIGATION OF THE CONCRETE SLAB FLOOR OF DISTRIBUTION WAREHOUSE

We conducted a crack survey of floor slabs in distribution warehouses up to 5 years old. As a result, the crack coefficient at 5 years of age was about 70 × 10-6 to 100 × 10-6 on the 2nd and 3rd floors, and about 30 × 10-6 on the 4th floor. The reason why the 4th floor is smaller than the other floo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:AIJ Journal of Technology and Design 2021/06/20, Vol.27(66), pp.618-621
Hauptverfasser: TSUZUKI, Masanori, FUKUDA, Kazuo, KOSHIRO, Yasumichi
Format: Artikel
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We conducted a crack survey of floor slabs in distribution warehouses up to 5 years old. As a result, the crack coefficient at 5 years of age was about 70 × 10-6 to 100 × 10-6 on the 2nd and 3rd floors, and about 30 × 10-6 on the 4th floor. The reason why the 4th floor is smaller than the other floors is that it is used less frequently than the other floors and is less affected by external forces such as vehicle running, and the slab is less restrained than the other floors.