Enhanced thermoelectric properties of (SnS)1−x(SnO)x: x ≤ 10.79% nanocomposites prepared by polyol method

(SnS) 1− x (SnO) x : x  = 0, 3.57%, 7.16%, and 10.79% nanocomposites (NCs) have been successfully synthesized using a simple polyol method. XRD data analysis shows formation of SnS and SnO NCs with an average crystallite size in the range from 30 to 35 nm. The Rietveld refinement analysis indicates...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials science. Materials in electronics 2021-04, Vol.32 (8), p.10702-10711
Hauptverfasser: Chotia, Chanderbhan, Tarachand, Okram, Gunadhor Singh, Kuo, Yung-Kang, Hussain, Shamima
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:(SnS) 1− x (SnO) x : x  = 0, 3.57%, 7.16%, and 10.79% nanocomposites (NCs) have been successfully synthesized using a simple polyol method. XRD data analysis shows formation of SnS and SnO NCs with an average crystallite size in the range from 30 to 35 nm. The Rietveld refinement analysis indicates layered orthorhombic crystal structure. FESEM images display the morphology of nanoflakes and nanoplates. Their positive Seebeck coefficients (α) suggest the p-type conduction. This is consistent with the deficiency of Sn found. (SnS) 0.9284 (SnO) 0.0716 NC exhibits a thermal conductivity ( κ ) of 0.75 Wm −1  K −1 at 300 K. Electrical (σ) and thermal conductivities are decreased, but α enhances with increasing x . Consequently, the dimensionless figure of merit (ZT) increases with increasing x up to 7.16% for which ZT at 325 K is 0.0036. This is 55% enhancement compared to the pure SnS that opens a new window for improvement of thermoelectric performance near room temperature.