Friction stir butt welding thin aluminum alloy sheets

0.8-mm-thick alclad 2024-T4 aluminum alloy sheets were friction stir butt welded. A 15-mm diameter shoulder tool was used to guarantee sufficient heat input during welding. A 0.08-mm shoulder plunge depth was adopted to reduce sheet thickness reduction. Sound joints were obtained at rotating speeds...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of advanced manufacturing technology 2018-06, Vol.96 (9-12), p.3139-3147
Hauptverfasser: Yue, Yumei, Wang, Guoqiang, Yang, Kang, Wu, Baosheng, Yan, Dejun
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:0.8-mm-thick alclad 2024-T4 aluminum alloy sheets were friction stir butt welded. A 15-mm diameter shoulder tool was used to guarantee sufficient heat input during welding. A 0.08-mm shoulder plunge depth was adopted to reduce sheet thickness reduction. Sound joints were obtained at rotating speeds from 400 to 1000 rpm and welding speeds from 50 to 150 mm/min. A thickness reduction of 6% was achieved at 1000 rpm and 50 mm/min. Secondary phases firstly precipitated at the black lines in the stir zone (SZ). The hardness of the SZ showed a decrease about 6% compared with the base metal. A maximum tensile strength of 399.5 MPa and an elongation of 5.6% were achieved at 1000 rpm and 150 mm/min. The fracture morphologies showed typical ductile fracture mode.
ISSN:0268-3768
1433-3015
DOI:10.1007/s00170-018-1798-z