Cyclic Aminosilane‐Based Additive Ensuring Stable Electrode–Electrolyte Interfaces in Li‐Ion Batteries

Ni‐rich cathodes are considered feasible candidates for high‐energy‐density Li‐ion batteries (LIBs). However, the structural degradation of Ni‐rich cathodes on the micro‐ and nanoscale leads to severe capacity fading, thereby impeding their practical use in LIBs. Here, it is reported that 3‐(trimeth...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Advanced energy materials 2020-04, Vol.10 (15), p.n/a
Hauptverfasser: Kim, Koeun, Hwang, Daeyeon, Kim, Saehun, Park, Sung O, Cha, Hyungyeon, Lee, Yoon‐Sung, Cho, Jaephil, Kwak, Sang Kyu, Choi, Nam‐Soon
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Ni‐rich cathodes are considered feasible candidates for high‐energy‐density Li‐ion batteries (LIBs). However, the structural degradation of Ni‐rich cathodes on the micro‐ and nanoscale leads to severe capacity fading, thereby impeding their practical use in LIBs. Here, it is reported that 3‐(trimethylsilyl)‐2‐oxazolidinone (TMS‐ON) as a multifunctional additive promotes the dissociation of LiPF6, prevents the hydrolysis of ion‐paired LiPF6 (which produces undesired acidic compounds including HF), and scavenges HF in the electrolyte. Further, the presence of 0.5 wt% TMS‐ON helps maintain a stable solid–electrolyte interphase (SEI) at Ni‐rich LiNi0.7Co0.15Mn0.15O2 (NCM) cathodes, thus mitigating the irreversible phase transformation from layered to rock‐salt structures and enabling the long‐term stability of the SEI at the graphite anode with low interfacial resistance. Notably, NCM/graphite full cells with TMS‐ON, which exhibit an excellent discharge capacity retention of 80.4%, deliver a discharge capacity of 154.7 mAh g−1 after 400 cycles at 45 °C. 3‐(Trimethylsilyl)‐2‐oxazolidinone as an electrolyte additive enables the high performance of Ni‐rich LiNi0.7Co0.15Mn0.15O2 (NCM)/graphite full cells by promoting the dissociation of LiPF6, scavenging HF, deactivating PF5, and constructing an electrochemically robust interface on the surface of the Ni‐rich NCM cathode, which prevents undesirable electrolyte decomposition, while vinylene carbonate aids the formation of a solid–electrolyte interphase to protect the graphite anode.