Solution Strengthening the Ti-6Al-4V Joints were Brazed by Ti-15Cu-15Ni and Ag-26.7Cu-4.5Ti Filler Foils

Using the optimal solution and aging treatment for Ti-6Al-4V brazed by Ti-15Cu-15Ni and Ag-26.7Cu-4.5Ti fillers, the average shear strengths of the lap-joint interface are improved. And the average grain sizes and the average lengths of Widmanstätten structure are significantly smaller than that of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2020-02, Vol.977, p.90-95
Hauptverfasser: Lee, Kuo Hsun, Yang, Sen Yeu
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Using the optimal solution and aging treatment for Ti-6Al-4V brazed by Ti-15Cu-15Ni and Ag-26.7Cu-4.5Ti fillers, the average shear strengths of the lap-joint interface are improved. And the average grain sizes and the average lengths of Widmanstätten structure are significantly smaller than that of post-brazed annealing. Both fillers specimens are examined to indicate the strengthening mechanism is to homogenize the microstructure of Ti-6Al-4V joints to simultaneously enhance the strength of joint braze and substrate.