S-doped activated mesoporous carbon derived from the Borassus flabellifer flower as active electrodes for supercapacitors

A successful transformation of Borassus flabellifer flower into activated carbon (AC) with the highest intakes of sulfur (S) contents in the S-doped AC process turned the materials to be a potential candidate for supercapacitor applications. The suitable proportion of KOH during activation and the e...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials chemistry and physics 2020-01, Vol.240, p.122151, Article 122151
Hauptverfasser: Maria Sundar Raj, F. Regan, Jaya, N. Victor, Boopathi, G., Kalpana, D., Pandurangan, A.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A successful transformation of Borassus flabellifer flower into activated carbon (AC) with the highest intakes of sulfur (S) contents in the S-doped AC process turned the materials to be a potential candidate for supercapacitor applications. The suitable proportion of KOH during activation and the effect of thiourea as a precursor were other major factors in the transformation process. Many experiments have left the possibility of the effects of the high S content of the materials unnoticed; this attempt explored the result of the high content S-doped mesoporous AC via hydrothermal method. Moreover, doping sulfur and oxygen functionalities on its carbon matrix helps to improve its electrochemical properties. HRSEM/EDX with elemental mapping evidenced the porous sheetlike morphologies. XRD, Raman spectra and nitrogen adsorption/desorption isotherm analysis were studied. The reported specific surface area of the AC (PM6) is found to be 474.99 m2/g with the highest 10 wt% of S at an activation temperature of 600 °C for 1 h with 30 wt% of KOH. This S-doped AC exhibits high specific capacitance of 275 F/g at a current density of 1 A/g. The symmetric supercapacitors cell (SSC) exhibited specific capacitance of 137.7 F/g at 1 A/g, with enhanced superior cycling stability with 95.4% retention after 3000 cycles at 1 A/g. The SSC delivers energy density of 9.345 Wh/kg and power density of 687 W/kg. [Display omitted] •Conversion of Borassus flabellifer flower into AC with the utmost intakes of S content.•Activation temperature 600 °C strongly influences enrich mesopores surface in the AC.•Palm male flower enhanced with the high capacitance of 275 F/g.•SSC delivers energy density of 9.345 Wh/kg and power density of 687 W/kg.
ISSN:0254-0584
1879-3312
DOI:10.1016/j.matchemphys.2019.122151