On the loss factor of wood during radio frequency heating
The radial direction loss factor of full-size western hemlock sapwood and heartwood, as well as western red cedar heartwood timbers was measured using the direct calorimetric method with a laboratory-scale radio frequency/vacuum dryer at the frequency of 13.56 MHz, moisture content range between 10...
Gespeichert in:
Veröffentlicht in: | Wood science and technology 1999-09, Vol.33 (4), p.299-310 |
---|---|
Hauptverfasser: | , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The radial direction loss factor of full-size western hemlock sapwood and heartwood, as well as western red cedar heartwood timbers was measured using the direct calorimetric method with a laboratory-scale radio frequency/vacuum dryer at the frequency of 13.56 MHz, moisture content range between 10 and 80%, temperature range between 25 and 55 degrees C, and root mean square (rms) electrode voltages of 0.8 and 1.1 kV, respectively. The results indicated that the moisture content, temperature, electric field strength and wood type significantly affected the loss factor. Empirical regression equations were derived based on the experimental data chat made possible the calculation of the loss factor and power density within wood during RF heating. |
---|---|
ISSN: | 0043-7719 1432-5225 |