The Detection and Characterization of Blisters On Carbon-Graphite Mechanical Seal Faces

Blisters that develop on carbon-graphite mechanical seal faces are irregularities in surface topography that result in poor sealing performance and a high incidence of catastrophic failure. On first inspection, a blister is a burnished area that is slightly elevated above the surrounding seal surfac...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Tribology transactions 2000-01, Vol.43 (3), p.395-402
Hauptverfasser: Guichelaar, Philip J., Wilde, Deborah A., Williams, Molly W.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Blisters that develop on carbon-graphite mechanical seal faces are irregularities in surface topography that result in poor sealing performance and a high incidence of catastrophic failure. On first inspection, a blister is a burnished area that is slightly elevated above the surrounding seal surface. In this study, the topography of several hundred blisters was examined with interference microscopy. The shape of the burnished area is typically elliptical or cylindrical. The leading edge against the direction of rotation of the mating seal ring extends abruptly upward from the surrounding seal surface. The trailing surface gradually merges into the parent seal face. Most blisters have a maximum height of 0.25 μm to 0.75 μm (10 μ-in to 30 μ-in). Presented at the 55th Annual Meeting Nashville, Tennessee May 7-11, 2000
ISSN:1040-2004