Mid-IR Cathodoluminescence of Fe:ZnSe

The dependences of the integral intensity and kinetics of mid-IR cathodoluminescence (CL) of Fe:ZnSe crystals on an iron concentration varying from 0.01 to 14 wt % are studied in the temperature range from 78 to 300 K. It is found that the maximum mid-IR CL intensity in Fe:ZnSe is observed at an Fe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Optics and spectroscopy 2018-12, Vol.125 (6), p.870-873
Hauptverfasser: Chukichev, M. V., Chegnov, V. P., Rezvanov, R. R., Chegnova, O. I., Kalinushkin, V. P., Gladilin, A. A.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The dependences of the integral intensity and kinetics of mid-IR cathodoluminescence (CL) of Fe:ZnSe crystals on an iron concentration varying from 0.01 to 14 wt % are studied in the temperature range from 78 to 300 K. It is found that the maximum mid-IR CL intensity in Fe:ZnSe is observed at an Fe concentration of about 2 wt % at room temperature and 0.8–1 wt % at liquid nitrogen temperature. A further increase in iron concentration leads to a decrease in the CL decay time.
ISSN:0030-400X
1562-6911
DOI:10.1134/S0030400X19020097