Porous Al^sub 2^O^sub 3^-Spinel Based Polycrystals That Resist Free-Sintering

We show that increasing MgO content in ... from 0.25 to 10 wt% has a remarkable effect on the sintering behavior. While 0.25 wt% specimens sinter to near full density, the higher weight percent sample could be sintered to a maximum of 92% relative density even when held for 24 h at 1673 K. The resis...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the American Ceramic Society 2008-10, Vol.91 (10), p.3451
Hauptverfasser: Shah, Sandeep R, Chokshi, Atul H, Raj, Rishi
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We show that increasing MgO content in ... from 0.25 to 10 wt% has a remarkable effect on the sintering behavior. While 0.25 wt% specimens sinter to near full density, the higher weight percent sample could be sintered to a maximum of 92% relative density even when held for 24 h at 1673 K. The resistance of the pores to sintering is ascribed to a reduction in the driving force for sintering (rather than to kinetics). The volume fraction of the pores increases with the fraction of the spinel phase, which forms by a reaction between magnesia and alumina. These findings raise the promise of membranes that can be tailored for pore size and pore volume, for high temperature applications. (ProQuest: ... denotes formulae/symbols omitted.)