Does the fatigue loading frequency affect the lithium disilicate glass ceramic inlay-dentin bond strength?

The aim of this study was to verify the effect of loading frequency during mechanical cycling on the microtensile bond strength between tooth and ceramic inlays. Twenty-four extracted permanent maxillary molars were standardly prepared (3 mm wide × 4 mm deep) to receive lithium disilicate-based cera...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of adhesion and adhesives 2018-08, Vol.84, p.301-306
Hauptverfasser: Trindade, Flavia Zardo, Campos, Fernanda, Marinho, Caroline Cotes, Bottino, Marco Antonio, Valandro, Luiz Felipe, Kleverlaan, Cornelis J.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The aim of this study was to verify the effect of loading frequency during mechanical cycling on the microtensile bond strength between tooth and ceramic inlays. Twenty-four extracted permanent maxillary molars were standardly prepared (3 mm wide × 4 mm deep) to receive lithium disilicate-based ceramic inlays. After the adhesive cementation, the restored teeth were divided into three groups (n = 8), according to different range of mechanical cycling frequency: control group – water storage, 2.0 Hz group – mechanical cycling at frequency of 2.0 Hz (0–100 N, 1.2 × 106 cycles, water 37 °C), and 6.7 Hz group – mechanical cycling at frequency of 6.7 Hz (0–100 N, 1.2 × 106 cycles, water 37 °C). The teeth were then cut into microbars (1 × 1 mm, non-trimming method), which were tested under microtensile (MTBS) loading. The failure mode was classified and the data were analyzed by one-way ANOVA. The mean bond strength value of the control group was the highest and the values of the cycled groups were 15% lower, however the groups were statistically similar (p = 0.58). Chi-square test showed no statistical difference among the groups regarding the pre-test failures (p = 0.17). For all groups, the most frequent failure type was mode 1 (adhesive at the interface ceramic/cement) and mode 2 (mixed failure). Loading frequencies up to 6.7 Hz had no effect on the lithium disilicate glass ceramic inlay-dentin bond strength.