Optimizing HIP and Printing Parameters for EBM Ti-6Al-4V

An investigation of HIP parameters for EBM Ti-6Al-4V has been performed with the aim to maximize the strength of the HIPed material. A lower HIP temperature of 800 °C and a higher pressure of 200 MPa gives the highest strength and is also enough to eliminate all internal defects. By printing materia...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Key engineering materials 2018-05, Vol.770, p.174-178
Hauptverfasser: Wedenstrand, Jouni, Ahlfors, Magnus, Eklund, Anders, Bahbou, Fouzi
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An investigation of HIP parameters for EBM Ti-6Al-4V has been performed with the aim to maximize the strength of the HIPed material. A lower HIP temperature of 800 °C and a higher pressure of 200 MPa gives the highest strength and is also enough to eliminate all internal defects. By printing material with intentionally induced porosity combined with an optimized HIP cycle the highest strength can be obtained.