Characterized the pattern of the material deposition in the HL-2A tokamak
Since the divertor geometry of a tokamak has a strong impact on the material erosion and deposition on the wall and HL-2A has a unique divertor configuration, it is necessary to investigate the material deposition pattern in HL-2A although a few results on other tokamaks have already been published....
Gespeichert in:
Veröffentlicht in: | Journal of nuclear materials 2017-03, Vol.485, p.67-73 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Since the divertor geometry of a tokamak has a strong impact on the material erosion and deposition on the wall and HL-2A has a unique divertor configuration, it is necessary to investigate the material deposition pattern in HL-2A although a few results on other tokamaks have already been published.
In this paper, tiles retrieved from the vessel are analyzed ex-situ by SIMS, SEM and laser-induced breakdown spectroscopy (LIBS). And deposition behind the lower divertor is in-situ measured by a quartz crystal microbalance (QMB). The deposition in HL-2A displays a complex pattern and clear localization characteristic. The thickness of the deposition layer varies in the range of 0-4μm. And in-situ diagnostic of QMB indicates that the average thickness of the deposition layer per pulse is over ten nanometers. In addition, the results imply that Si, Fe and D have different behaviors during the material deposition in HL-2A. |
---|---|