Preparation and proton conductivity of ultrafine Y-doped BaZrO3 ceramics

Y-doped BaZrO3 powders prepared by high-temperature solid state reactions often suffer the disadvantage of serious aggregation. In order to eliminate this disadvantage, planet-mill and sand-mill processing methods were employed. The results of particle-size determination and scanning electron micros...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the Ceramic Society of Japan 2017/06/01, Vol.125(6), pp.520-523
Hauptverfasser: YUANSHENG, Du, JINFENG, Xia, HONGQIANG, Nian, GUOHONG, Zhou, DANYU, Jiang, QIANG, Li
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Y-doped BaZrO3 powders prepared by high-temperature solid state reactions often suffer the disadvantage of serious aggregation. In order to eliminate this disadvantage, planet-mill and sand-mill processing methods were employed. The results of particle-size determination and scanning electron microscopy images confirm that sand milling can efficiently eliminate the aggregation and produce ultrafine and well-dispersed Y-doped BaZrO3 powders. Starting from powders treated by sand milling, completely densified Y-doped BaZrO3 ceramics can be fabricated by sintering at a low temperature of 1640°C for 15 h. Y-doped BaZrO3 ceramics sintered from powders treated by sand-mill for 5 h possess an ultrafine crystal size and a higher density and proton conductivity compared to those treated for 2 h.
ISSN:1882-0743
1348-6535
DOI:10.2109/jcersj2.17017