Effect of Alkali Treatment Using Calcium Hydroxide and the Fiber Length on the Strength of Sugarcane Bagasse Fibers-Polypropylene Composites

Milling sugarcanes to produce sugar generates by-product called bagasse. Due to the large availability and low cost, the potential of obtaining renewable and biodegradable fibers from bagasse had been explored. To produce fibers from these bagasse, the bagasse was treated in alkali solution using 14...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied Mechanics and Materials 2015-11, Vol.815, p.106-110
Hauptverfasser: Sugondo, Suwandi, Henrico, Steven, Anggono, Juliana, Purwaningsih, Hariyati
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Milling sugarcanes to produce sugar generates by-product called bagasse. Due to the large availability and low cost, the potential of obtaining renewable and biodegradable fibers from bagasse had been explored. To produce fibers from these bagasse, the bagasse was treated in alkali solution using 14 % v/v calcium hydroxide, Ca (OH)2 at high temperature (60-70°C) for 4 hours. After treatment and washed to remove dissolved substances, the fibers were cut into 3 and 5 cm length. Some fibers were prepared in their original length. These fibers were mixed with polypropylene (PP) matrix in weight % ratios of bagasse fibers/PP 20/80, 25/75, and 30/70 and hotpressed to make composite samples. Composites produced were characterised with tensile test to evaluate their tensile properties. Scanning electron microscopy (SEM) was performed on the fiber surface as well as on the fracture area of the tensile tested samples. Tensile strength of the composite shows an increase with the increase of the fiber length and weight % ratios of bagasse fibers/PP up to 25/75 and decreases when bagasse fibers were added to 30 wt.%. The highest strength of 11,30 MPa was obtained when 5 cm fibers were used in a weight % ratio of bagasse fibers/PP at 25/75. SEM study found a greater number of fibers oriented perpendicular to the tension direction.