Plastic buckling, wrinkling and collapse behaviour of dented X80 steel line pipes under axial compression

High strength steel pipes have found increasing applications in deep high pressure offshore oil/gas lines. Damages in the form of dent are among common causes of pipeline failure. Indentation, plastic buckling and residual strength of dented normal grade steel pipes under bending, axial and combined...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of loss prevention in the process industries 2015-11, Vol.38, p.67-78
Hauptverfasser: Zeinoddini, M., Ezzati, M., Parke, G.A.R.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:High strength steel pipes have found increasing applications in deep high pressure offshore oil/gas lines. Damages in the form of dent are among common causes of pipeline failure. Indentation, plastic buckling and residual strength of dented normal grade steel pipes under bending, axial and combined loading have previously been addressed by a number of researchers. The plastic buckling and collapse of dented high grades steel line pipes, however, have received less previous attentions. In the current study an experimental model testing was used to evaluate the residual strength of dented X80 steel pipes under monotonic axial compression. The tubular specimens were first laterally dented by an indentor while resting on a saddle shape support. The specimens were then examined under axial compression to study the dent effects on their collapse behaviour. Numerical simulations were also used to analyse the effect of the indentor ratio, shape and alignment on the residual strength of dented steel tubes under monotonic axial compression. The results from the current study on high strength steels were also compared with semi-empirical equations available in the literature for low strength steels. It was found that these equations provide reasonable predictions for the axial residual capacity of the high strength steel pipes when the dent depths are small. With deep dents, however, they considerably underestimate the axial residual capacity of the high strength steel pipes. •The behaviour of dented high strength steel tubulars under monotonic axial compressive loading has been studied.•The residual axial load bearing characteristics (FL, εL, Fchar.) decreased as the dent depth increased.•The results from the current study were also compared with semi-empirical equations.
ISSN:0950-4230
1873-3352
DOI:10.1016/j.jlp.2015.09.002