Experimental Study on the Displacement Performance of Heat-Resistant Polymer

The displacement performance of heat-resistant polymer is evaluated with the artificial cores and natural cores under 95°C. The best concentration of BH heat-resistant polymer is 1500 mg/L, and the best slug is 0.6 PV on the condition of the average permeability is 600×10-3μm2 of the homogeneous cor...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied Mechanics and Materials 2014-10, Vol.675-677, p.1495-1499
Hauptverfasser: Chen, Tao Ping, Qiu, Biao
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The displacement performance of heat-resistant polymer is evaluated with the artificial cores and natural cores under 95°C. The best concentration of BH heat-resistant polymer is 1500 mg/L, and the best slug is 0.6 PV on the condition of the average permeability is 600×10-3μm2 of the homogeneous core and the oil viscosity is 2.3mPa • s. Under the best concentration and the PV size, BH heat-resistant polymer solution has better displacement effect for the artificial double core whose permeability ratio is less than 4. When permeability ratio exceed 4, the displacement affect no longer increase. When the mobility ratio increase from 0.05 to 0.2, for the artificial cores, the recovery of polymer flooding reduce by 3.17%, and for the natural cores, the recovery of polymer flooding reduce by 2.26%. The recovery of BH polymer that is aged for 90 days after vacuumed is 32.29%. Comparing with the fresh BH polymer, it is lower by 6.56%. That is to say that the aged BH polymer still has good oil displacement efficiency.