Promoting Effect of Pd Addition to Ni0.2Mg0.8Al2O4 in Oxidative Steam Reforming of Methane
Addition of Pd to Ni0.2Mg0.8Al2O4 promoted oxidative steam reforming of methane, and it gave high activity under high partial pressure of steam and low W/F, where Ni0.2Mg0.8Al2O4 showed very low activity. The Ni0.2Mg0.8Al2O4 requires the H2 reduction pretreatment; however, Pd/Ni0.2Mg0.8Al2O4 can be...
Gespeichert in:
Veröffentlicht in: | Chemistry letters 2006-09, Vol.35 (9), p.1072-1073 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Addition of Pd to Ni0.2Mg0.8Al2O4 promoted oxidative steam reforming of methane, and it gave high activity under high partial pressure of steam and low W/F, where Ni0.2Mg0.8Al2O4 showed very low activity. The Ni0.2Mg0.8Al2O4 requires the H2 reduction pretreatment; however, Pd/Ni0.2Mg0.8Al2O4 can be activated automatically by the reactant gases of oxidative reforming of methane. |
---|---|
ISSN: | 0366-7022 1348-0715 |
DOI: | 10.1246/cl.2006.1072 |