Mechanical Properties of B4C-SiC Whisker Composite Ceramics
Composite ceramics of B4C containing up to 30vol% SiC whisker were fabricated by hot pressing at 2000°-2200°C under 30MPa for 30min. The mechanical properties (bending strength, fracture toughness, hardness, elastic modules) of the hot pressed bodies were measured. Fully dense B4C-SiC whisker compos...
Gespeichert in:
Veröffentlicht in: | Journal of the Ceramic Society of Japan 1990-01, Vol.98 (1142), p.1159 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Composite ceramics of B4C containing up to 30vol% SiC whisker were fabricated by hot pressing at 2000°-2200°C under 30MPa for 30min. The mechanical properties (bending strength, fracture toughness, hardness, elastic modules) of the hot pressed bodies were measured. Fully dense B4C-SiC whisker composite ceramics were obtained at the whisker contents up to 30vol% at a sintering temperature above 2100°C. These composites had maximum strength at the whisker content of 10 or 20vol% depending upon the hot pressing temperature. The composite containing 10vol% SiC whisker, fired at 2100°C, had the highest strength (about 830MPa), which was 40% larger than that of monolithic B4C. Slight increase of fracture toughness were obtained in the composites because there was no pull-out of whiskers and no crack deflection in the fracture process. The strength and fracture toughness of the composites containing whiskers with a small diameter were lower than those of the composites with a large diameter, since the whiskers with a small diameter could not maintain their original morphology after sintering. The hardness and elastic modulus were 30GPa and 430GPa, respectively, independent of whisker addition. |
---|---|
ISSN: | 1882-0743 1348-6535 |