Size-Controlled Synthesis of Magnetite Nanoparticles from Iron Acetate by Thermal Decomposition
Magnetite nanoparticles with an average particle size ranging from 4.2 to 34.2 nm were synthesized by thermal decomposition of iron(II) acetate with and without a reducing agent. While in the presence of reducing agent, magnetite nanopartices with an average size of 4.2 nm and 12.6 nm were synthesiz...
Gespeichert in:
Veröffentlicht in: | Applied Mechanics and Materials 2012-11, Vol.217-219, p.256-259 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Magnetite nanoparticles with an average particle size ranging from 4.2 to 34.2 nm were synthesized by thermal decomposition of iron(II) acetate with and without a reducing agent. While in the presence of reducing agent, magnetite nanopartices with an average size of 4.2 nm and 12.6 nm were synthesized by varying the amounts of the surfactants. While in the absence of the reducing agent, magnetite nanoparticles with an average size of 26.4 nm and 34.2 nm were prepared. |
---|---|
ISSN: | 1660-9336 1662-7482 1662-7482 |