Shape and Properties of Calcium Carbonate Obtained by Thermal Decomposition of Calcium Acetate

The production of calcium carbonate by the thermal decomposition of calcium acetate was tried. Calcium acetate changed into calcium carbonate (calcite structure) at a calcining temperature about 400°C. The particles were large and tabular polycrystalline aggregates of 0.3-1.4mm long and 0.06mm acros...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the Ceramic Society of Japan 1989-01, Vol.97 (1126), p.669
Hauptverfasser: MACHINAGA, Osamu, KASAI, Junichi
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The production of calcium carbonate by the thermal decomposition of calcium acetate was tried. Calcium acetate changed into calcium carbonate (calcite structure) at a calcining temperature about 400°C. The particles were large and tabular polycrystalline aggregates of 0.3-1.4mm long and 0.06mm across with low whiteness (under 40%), large oil absorption (95-110ml/100g) and small specific surface area (2-7m2/g).