Sintering of Ag-Pd in the Presence of a Reactive Glass

Sintering of an 80% Ag‐20% Pd powder in the absence of a liquid phase below 750°C proceeds according to a grain‐boundary diffusion model. The same powder was sintered with a glass which exhibited incomplete wetting. By comparing sintering rates, the occurrence of solution‐precipitation sintering in...