Biaxially textured Ni-alloy tapes as substrates for buffer and Y-Ba-Cu-O film growth

Highly cube ({001} ) textured Ni- and Ni-alloy tapes are produced by heavy cold rolling and recrystallisation annealing. Due to impurities in Ni, abnormal grain growth destroying the cube texture often occurs at temperatures above 600/spl deg/C. This could be prevented by alloying Ni with 0.1 at.% o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:IEEE transactions on applied superconductivity 2001-03, Vol.11 (1), p.3477-3480
Hauptverfasser: de Boer, B., Reger, N., Fernandez G.R., L., Eickemeyer, J., Berberich, P., Prusseit, W., Holzapfel, B., Schultz, L.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Highly cube ({001} ) textured Ni- and Ni-alloy tapes are produced by heavy cold rolling and recrystallisation annealing. Due to impurities in Ni, abnormal grain growth destroying the cube texture often occurs at temperatures above 600/spl deg/C. This could be prevented by alloying Ni with 0.1 at.% of different elements each leading to a texture improvement with increasing annealing temperature. YBa/sub 2/Cu/sub 3/O/sub 7-/spl delta//-films deposited on these tapes reach critical current densities up to 0.5/spl times/10/sup 6/ A/cm/sup 2/. Also Ni-Cr and Ni-V were successfully processed to highly cube textured tapes. Their magnetic and mechanical properties were characterized. Ni-13 at.% Cr and Ni-11 at.% V have a Curie temperature below 77 K. Their yield strength is three times higher than that of unalloyed Ni.
ISSN:1051-8223
1558-2515
DOI:10.1109/77.919812