Processing of fluxing underfills for flip chip-on-laminate assembly

Fluxing underfill eliminates process steps in the assembly of flip chip-on-laminate (FCOL) when compared to conventional capillary flow underfill processing. In the fluxing underfill process, the underfill is dispensed onto the board prior to die placement. During placement, the underfill flows in a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:IEEE transactions on electronics packaging manufacturing 2003-01, Vol.26 (1), p.75-83
Hauptverfasser: Zhao, R., Johnson, R.W., Jones, G., Yaeger, E., Konarski, M., Krug, P., Crane, L.L.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Fluxing underfill eliminates process steps in the assembly of flip chip-on-laminate (FCOL) when compared to conventional capillary flow underfill processing. In the fluxing underfill process, the underfill is dispensed onto the board prior to die placement. During placement, the underfill flows in a "squeeze flow" process until the solder balls contact the pads on the board. The material properties, the dispense pattern and resulting shape, solder mask design pattern, placement force, placement speed, and hold time all impact the placement process and the potential for void formation. A design of experiments was used to optimize the placement process to minimize placement-induced voids. The major factor identified was board design, followed by placement acceleration. During the reflow cycle, the fluxing underfill provides the fluxing action required for good wetting and then cures by the end of the reflow cycle. With small, homogeneous circuit boards it is relatively easy to develop a reflow profile to achieve good solder wetting. However, with complex SMT assemblies involving components with significant thermal mass this is more challenging.