Hall effect of sputtered NiZr and CoZr metallic glasses near the critical magnetic concentration

With increasing 3d component, the 3d transition-metal Zr amorphous alloys undergo a transition to ferromagnetism at xc=88 at. % Ni, 62 at. % Co, and 38 at. % Fe, respectively. The first two compositions are outside the range of stable melt-spun glasses, but can be prepared by sputtering. In this pap...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied physics 1990-05, Vol.67 (9), p.5790-5792
Hauptverfasser: MOREL, R, ABADLI, L, COCHRANE, R. W
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:With increasing 3d component, the 3d transition-metal Zr amorphous alloys undergo a transition to ferromagnetism at xc=88 at. % Ni, 62 at. % Co, and 38 at. % Fe, respectively. The first two compositions are outside the range of stable melt-spun glasses, but can be prepared by sputtering. In this paper, we present Hall data for sputtered NiZr and CoZr alloys in the vicinity of the critical magnetic composition. For the ferromagnetic glasses, x>xc, the alloys are magnetically soft. Although the NiZr alloys are quite weak magnetically [μ0M(T=0)=0.15 T at 90 at. %], the extraordinary Hall coefficient is very large (Rs=−0.67×10−7 m3/C for the same alloy). In the Co glasses, Rs is positive, but of the same magnitude even though the magnetism is considerably stronger. In the paramagnetic range x
ISSN:0021-8979
1089-7550
DOI:10.1063/1.345965