Quasi-two-dimensional electron gas at the interface of γ-Al{sub 2}O{sub 3}/SrTiO{sub 3} heterostructures grown by atomic layer deposition
We report the formation of a quasi-two-dimensional electron gas (2-DEG) at the interface of γ-Al{sub 2}O{sub 3}/TiO{sub 2}-terminated SrTiO{sub 3} (STO) grown by atomic layer deposition (ALD). The ALD growth of Al{sub 2}O{sub 3} on STO(001) single crystal substrates was performed at temperatures in...
Gespeichert in:
Veröffentlicht in: | Journal of applied physics 2015-09, Vol.118 (11) |
---|---|
Hauptverfasser: | , , , , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | We report the formation of a quasi-two-dimensional electron gas (2-DEG) at the interface of γ-Al{sub 2}O{sub 3}/TiO{sub 2}-terminated SrTiO{sub 3} (STO) grown by atomic layer deposition (ALD). The ALD growth of Al{sub 2}O{sub 3} on STO(001) single crystal substrates was performed at temperatures in the range of 200–345 °C. Trimethylaluminum and water were used as co-reactants. In situ reflection high energy electron diffraction, ex situ x-ray diffraction, and ex situ cross-sectional transmission electron microscopy were used to determine the crystallinity of the Al{sub 2}O{sub 3} films. As-deposited Al{sub 2}O{sub 3} films grown above 300 °C were crystalline with the γ-Al{sub 2}O{sub 3} phase. In situ x-ray photoelectron spectroscopy was used to characterize the Al{sub 2}O{sub 3}/STO interface, indicating that a Ti{sup 3+} feature in the Ti 2p spectrum of STO was formed after 2–3 ALD cycles of Al{sub 2}O{sub 3} at 345 °C and even after the exposure to trimethylaluminum alone at 300 and 345 °C. The interface quasi-2-DEG is metallic and exhibits mobility values of ∼4 and 3000 cm{sup 2} V{sup −1} s{sup −1} at room temperature and 15 K, respectively. The interfacial conductivity depended on the thickness of the Al{sub 2}O{sub 3} layer. The Ti{sup 3+} signal originated from the near-interfacial region and vanished after annealing in an oxygen environment. |
---|---|
ISSN: | 0021-8979 1089-7550 |