Post-test examination of a Li-Ta heat pipe exposed to H plasma in Magnum PSI
The authors exposed a radiatively cooled, Li-filled tantalum (Ta) heat pipe (HP) to a H plasma in Magnum PSI continuously for ˜2 h. We kept the overall heat load on the inclined HP constant and varied the tilt to give peak heat fluxes of ˜7.5–13 MW/m2. The peak temperature reached ˜1250 °C. This pap...
Gespeichert in:
Veröffentlicht in: | Fusion engineering and design 2019-09, Vol.146, p.2603-2607 |
---|---|
Hauptverfasser: | , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The authors exposed a radiatively cooled, Li-filled tantalum (Ta) heat pipe (HP) to a H plasma in Magnum PSI continuously for ˜2 h. We kept the overall heat load on the inclined HP constant and varied the tilt to give peak heat fluxes of ˜7.5–13 MW/m2. The peak temperature reached ˜1250 °C. This paper describes the post-test analysis and discusses Li HPs with materials other than Ta for fusion. A companion paper describes the experiment. |
---|---|
ISSN: | 0920-3796 1873-7196 |
DOI: | 10.1016/j.fusengdes.2019.04.053 |