니켈기 초내열합금 Alloy718의 고온 크리프 파단 특성

The short-term high temperature creep rupture behavior of Ni-based Alloy718 steel was investigated at the elevated temperatures range of 550 to $700^{\circ}C$ under constant stress conditions. The creep rupture characteristics such as creep stress, rupture time, steady state creep rate, and initial...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Han-guk haeyang gonghak hoeji (Online) 2008, 22(6), 85, pp.52-57
Hauptverfasser: 권상우(SANG-WOO KWON), 공유식(YU-SIK KONG), 김선진(SEON-JIN KIM)
Format: Artikel
Sprache:kor
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The short-term high temperature creep rupture behavior of Ni-based Alloy718 steel was investigated at the elevated temperatures range of 550 to $700^{\circ}C$ under constant stress conditions. The creep rupture characteristics such as creep stress, rupture time, steady state creep rate, and initial strain were evaluated. Creep stress has a quantitative correlation between creep rupture tim and steady state creep rate. The stress exponents (n, m) of the experimental data at 550, 600, 650 and $700^{\circ}C$ were derived as 33.5, -24.9, 26.1, -21.2, 16.8, -12.8 and 10, -8.2, respectively. The stress exponent decreased with increasing creep temperature. The creep lift prediction was derived by the Larson-Miller parameter (LMP) method and the resultant equation was obtained as follows: T($logt_r$+20)=-0.00252 ${\sigma}^2$-1.377${\sigma}$+-22718.
ISSN:1225-0767